| Item |
Unit |
TECHBARRIER -VAS |
Method |
| Thickness |
m |
12 |
JIS K 7130 |
| Haze |
% |
3.3 |
JIS K 7105 |
| Light Transmission Rate |
% |
89 |
JIS K 7105 |
| Tensile Strength |
MD |
MPa |
220 |
JIS K 7127 |
| TD |
230 |
| Elongation |
MD |
% |
150 |
JIS K 7127 |
| TD |
110 |
| COF |
SiOx/SiOx |
|
0.5 |
JIS K 7125 Type TR of TOYO-Seiki |
| SiOx/non-SiOx. |
0.4 |
| Surface specific resistance |
SiOx |
log / |
> 12 (> 12*1) |
JIS L 1094 |
| non-SiOx. |
> 11 (> 12*1) |
| Half time |
SiOx |
sec |
> 120 (> 120*1) |
JIS L 1094 |
| non-SiOx. |
> 10 (> 120*1) |
| Wet tension |
SiOx |
dyne/cm |
> 54 |
JIS L 1715 |
| non-SiOx. |
50 |
O2 Transmission rate 25 , 80%RH |
cc/(m2 d atm) |
0.7 |
MOCON Measured with laminated film |
Water vapor transmission rate 40 , 90%RH |
g/(m2 d) |
0.7 |
Bag Method Measured with laminated film |
*1 (data) show values of TECHBARRIER -V (standard type). Just comparison.
The above data is NOT guaranteed.
|