Property after retort with SUPERNYL -XT
| Item |
Unit |
Before |
After Retort 120 , 30 min |
| Thickness |
m |
15 |
- |
| Tensile Strength |
MPa {Kg/mm2} |
MD |
240 {24} |
240 {24} |
| TD |
280 {28} |
280 {28} |
| Elongation |
% |
MD |
120 |
120 |
| TD |
90 |
90 |
| Impact Strength |
J/piece {Kg-cm/piece} |
1.6 {16} |
1.6 {16} |
| Stick Strength |
N/piece {g/piece} |
5.2 {520} |
5.2 {520} |
| Oxygen Transmission rate |
fmol/(m2 s Pa) {cc/(m2 d atm)} |
40 {8} |
40 {8} |
| Water vapor Transmission rate |
g/(m2 d) |
100 |
100 |